Property |
Thickness |
Value |
Units |
Test |
OPTICAL
|
Haze |
142-300 |
0.4 |
% |
ASTM D1003 |
Haze |
400-500 |
0.6 |
% |
ASTM D1003 |
Haze |
700 |
0.8 |
% |
ASTM D1003 |
Haze |
1000 |
1.2 |
% |
ASTM D1003 |
Total Light Transmission (TLT) |
ALL |
90.5 |
% |
ASTM D1003 |
|
PHYSICAL
|
C.O.F. (dynamic) A-B |
142-1000 |
0.4 |
|
ASTM D1894 |
F5-MD |
142-1000 |
14,000 |
psi |
ASTM D882 |
F5-TD |
142-1000 |
14,000 |
psi |
ASTM D882 |
Tensile Strength MD |
142-1000 |
25,000 |
psi |
ASTM D882 |
Tensile Strength TD |
142-700 |
36,000 |
psi |
ASTM D882 |
Tensile Strength TD |
1000 |
30,000 |
psi |
ASTM D882 |
Yield (nominal) |
142 |
13,969 |
in˛/lb |
|
Yield (nominal) |
200 |
9,918 |
in˛/lb |
|
Yield (nominal) |
265 |
7,485 |
in˛/lb |
|
Yield (nominal) |
300 |
6,612 |
in˛/lb |
|
Yield (nominal) |
380 |
5,220 |
in˛/lb |
|
Yield (nominal) |
460 |
4,312 |
in˛/lb |
|
Yield (nominal) |
650 |
3,052 |
in˛/lb |
|
Yield (nominal) |
700 |
2,800 |
in˛/lb |
|
Yield (nominal) |
1000 |
1,984 |
in˛/lb |
|
|
THERMAL
|
Shrinkage MD (190°C) |
142-1000 |
2.5 |
% |
Unrestrained @ 190°C/5 min |
Shrinkage TD (190°C) |
142-1000 |
1.0 |
% |
Unrestrained @ 190°C/5 min |
|