Property |
Thickness |
Value |
Units |
Test |
OPTICAL
|
Haze |
48 |
3 |
% |
ASTM D1003 |
Haze |
92 |
4 |
% |
ASTM D1003 |
|
PHYSICAL
|
Elongation at Break MD |
48 |
130 |
% |
ASTM D882A |
Elongation at Break MD |
92 |
135 |
% |
ASTM D882A |
Elongation at Break TD |
48 |
100 |
% |
ASTM D882A |
Elongation at Break TD |
92 |
105 |
% |
ASTM D882A |
Tensile Modulus MD |
48 |
500,000 |
psi |
ASTM D882A |
Tensile Modulus MD |
92 |
500,000 |
psi |
ASTM D882A |
Tensile Modulus TD |
48 |
530,000 |
psi |
ASTM D882A |
Tensile Modulus TD |
92 |
540,000 |
psi |
ASTM D882A |
Tensile Strength MD |
48 |
25 |
kpsi |
ASTM D882A |
Tensile Strength MD |
92 |
25 |
kpsi |
ASTM D882A |
Tensile Strength TD |
48 |
30 |
kpsi |
ASTM D882A |
Tensile Strength TD |
92 |
30 |
kpsi |
ASTM D882A |
|
THERMAL
|
Shrinkage MD (150℃) |
48 |
1.5 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage MD (150℃) |
92 |
1.0 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage TD (150℃) |
48 |
0.5 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage TD (150℃) |
92 |
0.1 |
% |
Unrestrained @ 150℃/30 min |
|