Property |
Thickness |
Value |
Units |
Test |
BARRIER
|
Water Absorption |
300 - 1400 |
0.55 |
% |
ASTM D570-63 (1972), 1 week at 23℃ |
|
ELECTRICAL
|
Breakdown Voltage |
500 |
16 |
kV |
50 Hz continuously increasing at 500 V/sec, 6.3 mm electrodes |
Breakdown Voltage |
760 |
19 |
kV |
50 Hz continuously increasing at 500 V/sec, 6.3 mm electrodes |
Breakdown Voltage |
1000 |
23 |
kV |
50 Hz continuously increasing at 500 V/sec, 6.3 mm electrodes |
Breakdown Voltage |
1400 |
26 |
kV |
50 Hz continuously increasing at 500 V/sec, 6.3 mm electrodes |
Surface Resistivity |
300 - 1400 |
> 10^13 |
Ohms/sq |
ASTM D257, 500 V DC @ 20℃ 54% RH |
Volume Resistivity |
300 - 1400 |
10^15 |
log Ohm m |
100 V D.C. @ 25℃ for 100 sec |
|
PHYSICAL
|
C.O.F. (static) |
300 - 1400 |
0.30 |
|
ASTM D1894 |
Density |
300 - 1400 |
1.4 |
g/cc |
ASTM D1505 |
Elongation at Break MD |
300 - 1400 |
150 |
% |
ASTM D882A |
Elongation at Break TD |
300 - 1400 |
130 |
% |
ASTM D882A |
Oligomer Extraction |
300 - 1400 |
0.6 |
% |
24 hours boiling Xylene |
Tensile Strength MD |
300 - 1400 |
29.9 |
kpsi |
ASTM D882A |
Tensile Strength TD |
300 - 1400 |
31.3 |
kpsi |
ASTM D882A |
Yield (nominal) |
500 |
4,000 |
in²/lb |
|
Yield (nominal) |
760 |
2,600 |
in²/lb |
|
Yield (nominal) |
1000 |
2,000 |
in²/lb |
|
Yield (nominal) |
1400 |
1,400 |
in²/lb |
|
|