Property |
Thickness |
Value |
Units |
Test |
ELECTRICAL
|
Breakdown Voltage |
48 |
2.8 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
Breakdown Voltage |
75 |
3.5 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
Breakdown Voltage |
92 |
4.0 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
Breakdown Voltage |
142 |
5.5 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
Breakdown Voltage |
200 |
7.7 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
Breakdown Voltage |
300 |
10.0 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
Breakdown Voltage |
400 |
11.7 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
Breakdown Voltage |
500 |
13.5 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
|
OPTICAL
|
Haze |
48 |
3 |
% |
ASTM D1003 |
Haze |
75 |
5 |
% |
ASTM D1003 |
Haze |
92 |
16 |
% |
ASTM D1003 |
Haze |
142 |
18 |
% |
ASTM D1003 |
Haze |
200 |
24 |
% |
ASTM D1003 |
Haze |
300 |
29 |
% |
ASTM D1003 |
Haze |
400 |
37 |
% |
ASTM D1003 |
Haze |
500 |
43 |
% |
ASTM D1003 |
|
PHYSICAL
|
Elongation at Break MD |
48 |
110 |
% |
ASTM D882A |
Elongation at Break MD |
75 |
110 |
% |
ASTM D882A |
Elongation at Break MD |
92 |
110 |
% |
ASTM D882A |
Elongation at Break MD |
142 |
125 |
% |
ASTM D882A |
Elongation at Break MD |
200 |
135 |
% |
ASTM D882A |
Elongation at Break MD |
300 |
135 |
% |
ASTM D882A |
Elongation at Break MD |
400 |
140 |
% |
ASTM D882A |
Elongation at Break MD |
500 |
140 |
% |
ASTM D882A |
Elongation at Break TD |
48 |
70 |
% |
ASTM D882A |
Elongation at Break TD |
75 |
90 |
% |
ASTM D882A |
Elongation at Break TD |
92 |
90 |
% |
ASTM D882A |
Elongation at Break TD |
142 |
100 |
% |
ASTM D882A |
Elongation at Break TD |
200 |
110 |
% |
ASTM D882A |
Elongation at Break TD |
300 |
110 |
% |
ASTM D882A |
Elongation at Break TD |
400 |
115 |
% |
ASTM D882A |
Elongation at Break TD |
500 |
115 |
% |
ASTM D882A |
Tensile Strength MD |
48 |
26 |
kpsi |
ASTM D882A |
Tensile Strength MD |
75 |
28 |
kpsi |
ASTM D882A |
Tensile Strength MD |
92 |
28 |
kpsi |
ASTM D882A |
Tensile Strength MD |
142 |
28 |
kpsi |
ASTM D882A |
Tensile Strength MD |
200 |
28 |
kpsi |
ASTM D882A |
Tensile Strength MD |
300 |
27 |
kpsi |
ASTM D882A |
Tensile Strength MD |
400 |
26 |
kpsi |
ASTM D882A |
Tensile Strength MD |
500 |
27 |
kpsi |
ASTM D882A |
Tensile Strength TD |
48 |
32 |
kpsi |
ASTM D882A |
Tensile Strength TD |
75 |
34 |
kpsi |
ASTM D882A |
Tensile Strength TD |
92 |
34 |
kpsi |
ASTM D882A |
Tensile Strength TD |
142 |
34 |
kpsi |
ASTM D882A |
Tensile Strength TD |
200 |
33 |
kpsi |
ASTM D882A |
Tensile Strength TD |
300 |
31 |
kpsi |
ASTM D882A |
Tensile Strength TD |
400 |
30 |
kpsi |
ASTM D882A |
Tensile Strength TD |
500 |
30 |
kpsi |
ASTM D882A |
Yield (nominal) |
48 |
41,300 |
in²/lb |
|
Yield (nominal) |
75 |
26,500 |
in²/lb |
|
Yield (nominal) |
92 |
21,800 |
in²/lb |
|
Yield (nominal) |
142 |
14,000 |
in²/lb |
|
Yield (nominal) |
200 |
9,900 |
in²/lb |
|
Yield (nominal) |
300 |
6,600 |
in²/lb |
|
Yield (nominal) |
400 |
5,000 |
in²/lb |
|
Yield (nominal) |
500 |
4,000 |
in²/lb |
|
|
THERMAL
|
Shrinkage MD (150℃) |
48 |
2.0 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage MD (150℃) |
75 |
2.0 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage MD (150℃) |
92 |
1.9 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage MD (150℃) |
142 |
1.5 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage MD (150℃) |
200 |
1.3 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage MD (150℃) |
300 |
1.2 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage MD (150℃) |
400 |
1.1 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage MD (150℃) |
500 |
1.1 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage TD (150℃) |
48 |
1.0 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage TD (150℃) |
75 |
1.1 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage TD (150℃) |
92 |
1.1 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage TD (150℃) |
142 |
1.0 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage TD (150℃) |
200 |
0.8 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage TD (150℃) |
300 |
0.8 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage TD (150℃) |
400 |
0.7 |
% |
Unrestrained @ 150℃/30 min |
Shrinkage TD (150℃) |
500 |
0.7 |
% |
Unrestrained @ 150℃/30 min |