| Property |
Thickness |
Value |
Units |
Test |
|
ELECTRICAL
|
| Breakdown Voltage |
750 |
17.5 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
| Breakdown Voltage |
900 |
18.4 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
| Breakdown Voltage |
1000 |
19.0 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
| Breakdown Voltage |
1400 |
20.0 |
kV |
ASTM D149 1/4" electrode 500 V/sec 25℃ in air |
|
|
|
OPTICAL
|
| Opacity |
750 |
38 |
% |
optical density |
| Opacity |
900 |
41 |
% |
optical density |
| Opacity |
1000 |
42 |
% |
optical density |
| Opacity |
1400 |
46 |
% |
optical density |
|
|
|
PHYSICAL
|
| Density |
750 |
1.3928 |
g/cc |
|
| Density |
900 |
1.3920 |
g/cc |
|
| Density |
1000 |
1.3925 |
g/cm3 |
|
| Density |
1400 |
1.3925 |
g/cc |
|
| Elongation at Break MD |
750 |
140 |
% |
ASTM D882A |
| Elongation at Break MD |
900 |
150 |
% |
ASTM D882A |
| Elongation at Break MD |
1000 |
150 |
% |
ASTM D882A |
| Elongation at Break MD |
1400 |
170 |
% |
ASTM D882A |
| Elongation at Break TD |
750 |
115 |
% |
ASTM D882A |
| Elongation at Break TD |
900 |
130 |
% |
ASTM D882A |
| Elongation at Break TD |
1000 |
140 |
% |
ASTM D882A |
| Elongation at Break TD |
1400 |
170 |
% |
ASTM D882A |
| Tensile Strength MD |
750 |
27 |
kpsi |
ASTM D882A |
| Tensile Strength MD |
900 |
27 |
kpsi |
ASTM D882A |
| Tensile Strength MD |
1000 |
27 |
kpsi |
ASTM D882A |
| Tensile Strength MD |
1400 |
26 |
kpsi |
ASTM D882A |
| Tensile Strength TD |
750 |
30 |
kpsi |
ASTM D882A |
| Tensile Strength TD |
900 |
29 |
kpsi |
ASTM D882A |
| Tensile Strength TD |
1000 |
29 |
kpsi |
ASTM D882A |
| Tensile Strength TD |
1400 |
25 |
kpsi |
ASTM D882A |
| Yield (nominal) |
750 |
2,600 |
in²/lb |
|
| Yield (nominal) |
900 |
2,200 |
in²/lb |
|
| Yield (nominal) |
1000 |
2,000 |
in²/lb |
|
| Yield (nominal) |
1400 |
1,400 |
in²/lb |
|
|
|
|
THERMAL
|
| Shrinkage MD (150℃) |
750 |
1.6 |
% |
Unrestrained @ 150℃/30 min |
| Shrinkage MD (150℃) |
900 |
1.6 |
% |
Unrestrained @ 150℃/30 min |
| Shrinkage MD (150℃) |
1000 |
1.5 |
% |
Unrestrained @ 150℃/30 min |
| Shrinkage MD (150℃) |
1400 |
1.3 |
% |
Unrestrained @ 150℃/30 min |
| Shrinkage TD (150℃) |
750 |
0.9 |
% |
Unrestrained @ 150℃/30 min |
| Shrinkage TD (150℃) |
900 |
1.1 |
% |
Unrestrained @ 150℃/30 min |
| Shrinkage TD (150℃) |
1000 |
1.1 |
% |
Unrestrained @ 150℃/30 min |
| Shrinkage TD (150℃) |
1400 |
0.8 |
% |
Unrestrained @ 150℃/30 min |