Property |
Thickness |
Value |
Units |
Test |
BARRIER
|
Gas Permeability - O2, 24 hr |
48 |
6 |
cc/100 in² |
ASTM D1434 77℉/75% RH/1 ATM |
WVTR |
48 |
2.8 |
g/100 in²/day |
ASTM F1249 38℃, 90% RH |
|
OPTICAL
|
Haze |
200 |
8.8 |
% |
ASTM D1003 |
Haze |
48 |
3.8 |
% |
ASTM D1003 |
Haze |
92 |
5.7 |
% |
ASTM D1003 |
|
PHYSICAL
|
C.O.F. (dynamic) |
48-200 |
0.4 |
|
ASTM D1894 |
C.O.F. (static) |
48 |
0.5 |
|
ASTM D1894 |
Density |
48-200 |
1.40 |
g/cc |
|
Elongation at Break MD |
200 |
150 |
% |
ASTM D882A |
Elongation at Break MD |
48 |
110 |
% |
ASTM D882A |
Elongation at Break MD |
92 |
130 |
% |
ASTM D882A |
Elongation at Break TD |
200 |
110 |
% |
ASTM D882A |
Elongation at Break TD |
48 |
70 |
% |
ASTM D882A |
Elongation at Break TD |
92 |
90 |
% |
ASTM D882A |
Tensile Strength MD (break) |
48-200 |
28,500 |
psi |
ASTM D882A |
Tensile Strength TD (break) |
200 |
33,000 |
psi |
ASTM D882A |
Tensile Strength TD (break) |
48 & 92 |
36,000 |
psi |
ASTM D882A |
|
THERMAL
|
Shrinkage MD (190℃) |
48-200 |
3 |
% |
Unrestrained @ 190℃/5 min |
Shrinkage TD (190℃) |
200 |
0.6 |
% |
Unrestrained @ 190℃/5 min |
Shrinkage TD (190℃) |
48 & 92 |
1.3 |
% |
Unrestrained @ 190℃/5 min |
|