Property |
Thickness |
Value |
Units |
Test |
OPTICAL
|
Haze |
500 |
0.5 |
% |
ASTM D1003 |
Haze |
700 |
1.0 |
% |
ASTM D1003 |
Haze |
1000 |
1.0 |
% |
ASTM D1003 |
|
PHYSICAL
|
Elongation at Break MD |
500 |
206 |
% |
ASTM D882A |
Elongation at Break MD |
700 |
217 |
% |
ASTM D882A |
Elongation at Break MD |
1000 |
200 |
% |
ASTM D882A |
Elongation at Break TD |
500 |
119 |
% |
ASTM D882A |
Elongation at Break TD |
700 |
132 |
% |
ASTM D882A |
Elongation at Break TD |
1000 |
120 |
% |
ASTM D882A |
Tensile Strength MD |
500 |
28,700 |
psi |
ASTM D882A |
Tensile Strength MD |
700 |
28,200 |
psi |
ASTM D882A |
Tensile Strength MD |
1000 |
26,000 |
psi |
ASTM D882A |
Tensile Strength TD |
500 |
29,200 |
psi |
ASTM D882A |
Tensile Strength TD |
700 |
31,300 |
psi |
ASTM D882A |
Tensile Strength TD |
1000 |
27,000 |
psi |
ASTM D882A |
|
THERMAL
|
Shrinkage MD (190℃) |
500 |
2.4 |
% |
Unrestrained @190℃/5 min |
Shrinkage MD (190℃) |
700 |
2.4 |
% |
Unrestrained @190℃/5 min |
Shrinkage MD (190℃) |
1000 |
2.4 |
% |
Unrestrained @ 190℃/5 min |
Shrinkage TD (190℃) |
500 |
1.2 |
% |
Unrestrained @190℃/5 min |
Shrinkage TD (190℃) |
700 |
1.0 |
% |
Unrestrained @190℃/5 min |
Shrinkage TD (190℃) |
1000 |
1.0 |
% |